How much Pentacryl does it take to absorb all the way through wood?

The amount of Pentacryl the wood will absorb depends upon the type of wood. For very dense grained hardwoods, it will take as little as 1 ounce per board foot and for very soft open grained wood it will take as much as 8 ounces per board foot. There is a wood calculator on our website to help determine the amount needed: Wood Calculator.